Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 14.0 g/10 min | 14.0 g/10 min | ASTM D1238 |
S&E Specialty Polymers TufGuard M™ GPP1005M-EXLT PP, Flame Retardant Application: UL94 V-2, Non-blooming flame retardant polypropylene compound for injection molding.Information provided by S&E Specialty Polymers |
|||
Melt Flow | 14.0 - 64.0 g/10 min | 14.0 - 64.0 g/10 min | Average value: 39.7 g/10 min Grade Count:8 |
Overview of materials for PET + PBT Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Melt Flow | 14.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
14.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Elexar® EL 3954-70 Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
Melt Flow | 14.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
14.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Elexar® EL 3954-90 Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
Melt Flow | 14.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
14.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1320E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 14.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
14.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1358C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 14.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
14.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2374A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 14.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
14.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-3955B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 14.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
14.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW2492 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (700000 ppm) Uses: Film; Sheet Forms: Pellets Processing Method: Injection Molding;.. |
|||
Melt Flow | 14.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
14.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 4975F Thermoplastic Elastomer Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T.. |
|||
Melt Flow | 14.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
14.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1431B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 14.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
14.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Terraloy™ MB 18003A Thermoplastic Starch + HIPS Notes: Terraloy™ MB-18003A is a Thermoplastic Starch/HIPS masterbatch that contains up to 30% of TPS renewable content. High Impact PS Melt Index for the masterbatch is 9.8. This compound is inte.. |
|||
Melt Flow | 14.0 g/10 min @Load 2.16 kg, Temperature 200 °C |
14.0 g/10 min @Load 4.76 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Uniprene® UN-1011A Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Flow | 14.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
14.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-8732 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 14.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
14.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-8732R Thermoplastic Elastomer Notes: RoHS Compliant Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstri.. |
|||
Melt Flow | 14.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
14.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron HI40I ABS Injection Molding Grade Automotive applications -Super High Impact , High Rigidity, PaintableInformation provided by Bhansali |
|||
Melt Flow | 14.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
14.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Elexar® EL 3954-80 Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical properti.. |
|||
Melt Flow | 14.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
14.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron HI40I ABS Injection Molding Grade Automotive applications -Super High Impact , High Rigidity, PaintableInformation provided by Bhansali |