Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 12.63 g/10 min | 12.63 g/10 min | ISO 1133 |
Styrolution Styrolux® 693 D SBC Description: Styrolux® 693 D is a clear styrene-butadiene copolymer (SBC) with a well balanced combination of toughness and clarity. Styrolux® 693 D is mainly used for thermoformed articles, e.. |