Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | ASTM D1238 |
Plaskolite Optix® CA-1000 IG Clear High Impact Acrylic Resin High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin offers the best impact resista.. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | ASTM D1238 |
Plaskolite West Optix® CA-1000 IG UC Clear High Impact Acrylic Resin High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin is suited for Gamma irradiatio.. |
|||
Melt Flow | 1.6 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.6 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CP - 86 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | |
DuPont Fusabond® MN493D Ethylene Octene Copolymer
(discontinued **) Typical Use: Nylon 6 toughenerNylon 6/6 toughenerComplies to FDA 21CFR 175.105Availability: North AmericaInformation provided by DuPont. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | Condition G |
Ineos Nova 1280 High Heat Crystal Polystyrene
(discontinued **) Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | ExxonMobil Method |
ExxonMobil LD 117.03 Blown Overwrap Film Resin
(discontinued **) LD 117 resins are homopolymer film resins with good clarity and excellent stiffness. Film from LD 117 resins can be used in overwrap applications and push-through type packaging equipment. Film ma.. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-117 MDPE Blown Overwrap Film Resin, Tough
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-117 can be used in overwrap applications and in push-through .. |
|||
Melt Flow | 1.6 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.6 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
M. Holland Company PP100 Polypropylene Homopolymer, General Purpose High clarityHomopolymerGood melt strengthHigh tensile strengthApplications: Thin-walled partsSheetStrapping |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | Condition G |
Ineos Nova 1290 High Heat Crystal Polystyrene Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | ISO 1133 |
Lucite International Diakon® CLH952 Acrylic Polymer Information provided by Lucite International |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | ASTM D1238 |
Lucky CF-920 Acrylic May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability. |
|||
Melt Flow | 1.6 g/10 min @Load 6.60 kg, Temperature 295 °C |
1.6 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM LTX300B PEI (Asia Pacific) Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | ISO 1133 |
Solvay Specialty Polymers Polidan® PNT 0555/06 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0555/06 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes... |
|||
Melt Flow | 1.6 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.6 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Borcoat™ BB700E-7032 Polypropylene Compound for Steel Pipe Coating Applications Borcoat BB700E-7032 is a grey colored high impact polypropylene. This product is especially designed for direct extrusion of syntactic PP with high thermal insulations capacity and high compression.. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | ASTM D1238L |
Total PPH 3230 Polypropylene, Blow Molding Grade Homopolymer blow molding gradeLubricated - Fina 3230 offers superior core rod release, eliminating the need for additional lubricant.High Purity - Fina 3230 features minimum taste and odor and optim.. |
|||
Melt Flow | 1.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LD 117.85 Blown Overwrap Film Resin Product Description: LD 117.85 is a homopolymer film resin with good clarity and excellent stiffness. Film made from LD 117.85 resin can be used in overwrap applications and in push-through type pac.. |
|||
Melt Flow | 1.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 117.85 Low Density Polyethylene Resin Product Description: LD 117.85 is a homopolymer film resin with good clarity and excellent stiffness. Film made from LD 117.85 resin can be used in overwrap applications and in push-through type pac.. |
|||
Melt Flow | 1.6 g/10 min @Load 2.16 kg |
1.6 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 10.2. |
Dow AFFINITY™ PF 1140 Polyolefin Plastomer AFFINITY® PF 1140 polyolefin plastomer is an ethylene alpha-olefin resin designed for use in a variety of demanding applications including high-speed, form-fill seal products, display films and fre.. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | ASTM D1238 |
Dow AFFINITY™ PF 1140G Polyolefin Plastomer (POP) AFFINITY™ PF 1140G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed to be used in a variety of demanding applications including form-fill-seal packaging and fre.. |
|||
Melt Flow | 1.6 g/10 min @Load 2.16 kg, Temperature 235 °C |
1.6 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AESN Y T6L Nylon 12, MoS2 Filled (Dry) Designation ISO 1874-PA12,EHLS,22-010,MD05Grade with molybdenum filler for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Low friction coefficient. No need of l.. |
|||
Melt Flow | 1.6 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.6 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem TI4015F Impact Copolymer Polypropylene Description: Superior balance of stiffness and impact strength. Applications: Suggested uses include extrusion applications requiring good impact strength. Process: Extrusion. This resin meets the .. |
|||
Melt Flow | 1.6 g/10 min @Load 2.16 kg, Temperature 235 °C |
1.6 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AESN Y T6L Nylon 12, MoS2 Filled (Conditioned) Designation ISO 1874-PA12,EHLS,22-010,MD05Grade with molybdenum filler for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Low friction coefficient. No need of l.. |
|||
Melt Flow | 1.6 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.6 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Arkema Group Solarkote® A200 Acrylic Superior UV protection and weatherability, ASTM Classification PMMA 0233V1Information provided by Arkema Group |
|||
Melt Flow | 1.6 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.6 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CP - 86 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | ASTM D1238 |
Plaskolite West Optix® CA-1000 IG Clear High Impact Acrylic Resin High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin is suited for Gamma irradiatio.. |
|||
Melt Flow | 1.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
condition E; ASTM D1238 |
DuPont™ Surlyn® 9730 Ionomer Resin, Zinc
(discontinued **) Surlyn® 9730 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | Exxon Method |
ExxonMobil Iotek® 8020 Sodium Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A sodium ionomer with excellent abrasion resistance, impact strength, hardness and tensile strength. IOTEK ionomers provide superb low temperature .. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | Condition G |
Ineos Nova 1200 High Heat Crystal Polystyrene Good processing characteristics, High tensile strength and modulus, Excellent clarity, USP Class VIApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radia.. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | Condition G |
Ineos Nova 1204 High Heat Crystal Polystyrene Good processing characteristics, High tensile strength and modulus, Excellent clarity, USP Class VIApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radia.. |