Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.96 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.96 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 58G (High Gloss) HDPE Blow Molding Resin
(discontinued **) Features: Outstanding gloss, pearlescent finish when colored, good processability.Applications: Small part blow molding, injection blow molding, low-moderate ESCR uses.Data provided by the manufactu.. |
|||
Melt Flow | 0.96 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.96 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 14L1 Octene LMDPE Film Resin
(discontinued **) Low gel, Good clarity, Excellent sealing characteristicsApplications: Lamination, Co-extrusionAdditives: Process stabilizer, polymer process aidFilm properties are typical of blown film extruded at .. |
|||
Melt Flow | 0.96 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.96 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Arkema Group Evatane® 1005 VN 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for films with high transparency and high mechanical properties. Examples: coextrusion, stretch film, paper-stationary, fancy .. |