Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Nylex™ 1230 Natural Polyamide + PP Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing.. |
|||
Melt Flow | 0.95 g/10 min @Load 21.6 kg, Temperature 190 °C |
0.95 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D 1238 |
NOVA Chemicals Sclair® 19C (High Gloss) HDPE Blow Molding Resin 19C complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without te.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 19C Homopolymer HDPE Film Resin Film Properties. Features: Good stiffness, good barrier, high clarity, narrow MWD.Applications: Lamination, co-extrusion.Data provided by the manufacturer. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 12J1 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity.Applications: Overwrap, lamination.Data provided by the manufacturer. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Montell 12C01G2 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, no antiblockApplications: f.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Montell 12C01G3 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, low antiblockApplications: .. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Montell 12C01G4 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, high slip, medium antiblockApplicati.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Montell 12C01G5 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, very high slip, medium antiblockAppl.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Montell 16501F4 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets F.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Montell 16501F6 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets .. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Montell 16501F7 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Montell 16501F8 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical LUTENE CCO550BK PE Compound Description: LUTENE CC0550BK offer the following properties: high mechanical properties, good environmental stress cracking resistance, excellent wetherability and high speed extrusion to give a smo.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L42009F Film (Butene Grade) LLDPE Extra High Molecular Weight Hexene Copolymer Formolene® L42009F is a general-purpose film grade linear low density made using gas-phase technology. The resin exhibits excellent toughness and streng.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L42009H Film (Butene Grade) LLDPE Butene Copolymer (Barefoot/with high AO)Applications: Higher AO package for cast and stretch filmHigher AO package for cast and stretch filmMeets all requirements of the U.S. Food and Drug Administr.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L42009PE Film (Butene Grade) LLDPE Linear Low Density Polyethylene Butene Copolymer for Film Extrusion Formolene® L42009PE is a general-purpose film grade linear low density made using gas-phase technology. The resin exhibits excell.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L62009A Film (Hexene Grade) LLDPE Hexene Copolymer (High Antiblock)Applications: Blown film applications that don’t require slip.Blown film applications that don’t require slip.Meets all requirements of the U.S. Food and Drug Admi.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L62009E2 Film (Hexene Grade) LLDPE Hexene Copolymer (High slip and antiblock)Applications: Blown film, general purpose filmBlown film, general purpose filmMeets all requirements of the U.S. Food and Drug Administration as specified i.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L62009H Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Higher AO package for cast and stretch filmHigher AO package for cast and stretch filmMeets all requirements of the U.S. Food and Drug Administration as spec.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis VL5580 High Density Polyethylene VL5580 is a high density polyethylene. This grade is especially designed for monofilament and cast film stretch tape production. Applications: ropes, twines , nets, monofilament applications, stra.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L42009A Film (Butene Grade) LLDPE Butene Copolymer (High Antiblock)Applications: Blown file for either blending or extrusionBlown file for either blending or extrusionMeets all requirements of the U.S. Food and Drug Administration a.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L42009B Film (Butene Grade) LLDPE Butene Copolymer (Barefoot)Applications: Blown file for either blending or extrusionBlown file for either blending or extrusionMeets all requirements of the U.S. Food and Drug Administration as spec.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L42009E2 Film (Butene Grade) LLDPE Butene Copolymer (Low slip and antiblock)Applications: Blown filmBlown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyo.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L42009M Film (Butene Grade) LLDPE Butene Copolymer (High slip and antiblock)Applications: Blown filmBlown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of poly.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L62009B Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Blown filmBlown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L62009X Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Cross laminated filmCross laminated filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg |
0.95 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 8. |
Dow DOWLEX™ NG 2085 Linear Low Density Polyethylene, Ethylene-Octene Copolymer Next Generation DOWLEX® NG 2085 resin is an ethylene-octene copolymer offering superior impact and tensile strength for down-gauged consumer liner film applications. It complies with U.S. FDA regul.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 11J1 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent hermetic heat sealability, easy processability, high toughness and strength.Applications: Sealant web in food packaging, vacuum packaging, barrier appl.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 11J4 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent hermetic heat sealability, easy processability, high toughness and strength.Applications: Sealant web in food packaging, vacuum packaging, barrier appl.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 13J7 Octene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity.Applications: Film.Data provided by the manufacturer. |