Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Riblene® FC 30 Low Density Polyethylene - Blown Film Extrusion Riblene FC 30 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 30 is characterized by a high melt strength leading to a good bubble sta.. |
|||
Melt Flow | 0.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Riblene® FC 40 Low Density Polyethylene - Blown Film Extrusion Riblene FC 40 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 40 is characterized by a high melt strength leading to a good bubble stability.. |
|||
Melt Flow | 0.27 g/10 min | 0.27 g/10 min | ISO 1133 |
Total Lacqtene® FB 3010 LDPE blown film
(discontinued **) Low density radical polyethylene made by high pressure autoclave. Advised temperature profile : 180 to 220°C.Information provided provided by Total Petrochemicals.Total Petrochemicals includes form.. |
|||
Melt Flow | 0.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips HiD® 9406 HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Good Parison Uniformity, Good Stress Crack ResistanceAppli.. |
|||
Melt Flow | 0.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips HiD® 9502/HiD® 9503 with Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Excellent ESCR, High Melt Strength, Good Impact Resistance.. |
|||
Melt Flow | 0.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips HiD® 9506 HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Good ESCR, High Melt Strength, Good Impact Resistance, Goo.. |
|||
Melt Flow | 0.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips HiD® 9330 HDPE Natural Pipe Resin
(discontinued **) Resin Type: gas phase linear hexane copolymer; ASTM D3350 Classification 335520A; ASTM D4976 Classification: PE 235, A 55701Applications: base resin for use in utility and conduit pipe applicationsI.. |
|||
Melt Flow | 0.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips HiD® 9502H - 9503H High Performance Series HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: outstanding ESCR, excellent impact resistance, medium molecular weight distribution, wide range of processing conditions, high melt strength, good pariso.. |
|||
Melt Flow | 0.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips Marlex® 9506H High Performance Series HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: superior physical properties, medium molecular weight distribution, wide range of processing conditions, low parison sag, excellent stress crack resistan.. |
|||
Melt Flow | 0.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 16A Butene HDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good barrier properties.Applications: Merchandising bags, lamination, co-extrusion.Data provided by the manufacturer. |
|||
Melt Flow | 0.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 14A Butene MDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, strength and toughness, broad MW distribution.Applications: Co-extrusion, blending.Data provided by the manufacturer. |
|||
Melt Flow | 0.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos G36-24-149 MDPE with Carbon Black
(discontinued **) Fortiflex® G36-24-149 is a black medium density polyethylene resin designed for sheet extrusion. This resin has excellent environmental stress crack resistance (ESCR) and ultra violet protection. .. |
|||
Melt Flow | 0.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos G36-24-150 HDPE Ineos G36-24-150 is a medium density polyethylene resin designed for geomembrane sheet extrusion. The resin has excellent environmental stress crack resistance (ESCR).Natural resin; some physical p.. |
|||
Melt Flow | 0.27 g/10 min @Load 2.16 kg |
0.27 g/10 min @Load 4.76 lb |
ISO 1133 |
Total Xsene® BM 593 HDPE, blow molding FINATHENE® BM 593 is a new generation of bimodal high density polyethylene based on hexene (C6) as co-monomer and is produced by the ATOFINA Double Loop Technology™. FINATHENE® BM 593 has been es.. |
|||
Melt Flow | 0.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips Marlex® 9503HF High Performance Series HDPE Blow Molding Resin Resin Type: linear copolymerCharacteristics: outstanding ESCR, excellent impact resistance, medium molecular weight distribution, wide range of processing conditions, high melt strength, good pariso.. |
|||
Melt Flow | 0.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem TS7003 LDPE Blown Film Extrusion Polyethylene TS7003 is a low-density polyethylene (LDPE) with high molecular weight that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily processed. Th.. |
|||
Melt Flow | 0.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips HiD® 9330T HDPE Natural Pipe Resin
(discontinued **) Resin Type: Gas Phase Linear Hexene CopolymerASTM D 4976 Classification: PE 235, A 54607ASTM D3350 Classification: 335540AApplications: Base resin for use in utility and conduit pipe applications.Da.. |
|||
Melt Flow | 0.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem TS9003 LDPE Blown Film Extrusion Polyethylene TS9003 is a low-density polyethylene (LDPE) that presents excellent mechanical resistance along with good optical properties and high stiffness. These characteristics ensure the production of packag.. |
|||
Melt Flow | 0.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem TX7003 LDPE Blown Film Extrusion Polyethylene TX7003 is a low-density, high molecular-weight polyethylene that offers high mechanical strength. The product's characteristics allow for high versatility and use in various applications due to its .. |