Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 60 SUS | 60 SUS | |
ConocoPhillips Syncon® 68 Synthetic AW Hydraulic Fluid 68 Description: Conoco Syncon Synthetic AW Hydraulic Fluid is a synthetic polyalphaolefin (PAO) antiwear fluid for hydraulic systems that operate at extreme temperatures. It is available in four ISO vi.. |
|||
Saybolt Viscosity at 210°F | 60 SUS | 60 SUS | |
ChevronTexaco Drive Train Fluid HD, SAE 30 FeaturesChevron Drive Train Fluids HD are high performance lubricants designed for use in transmissions, final drives, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or Allison C4 .. |
|||
Saybolt Viscosity at 210°F | 60 SUS | 60 SUS | |
ChevronTexaco Tool Joint Compound FeaturesChevron Tool Joint Compound is an aluminum complex grease designed principally for the lubrication of drill collars, tool joints and pipe threads.It contains copper flake and graphite, forti.. |
|||
Saybolt Viscosity at 210°F | 60 SUS | 60 SUS | ASTM D-2161 |
ConocoPhillips ANDEROL® 6068 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Saybolt Viscosity at 210°F | 60 SUS | 60 SUS | |
ConocoPhillips Hydroclear® MV68 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Saybolt Viscosity at 210°F | 60 SUS | 60 SUS | |
ChevronTexaco Biostar® Hydraulic 46 Texaco Biostar Hydraulic oils deliver value through:Environmental sensitivity — Readily biodegradable formulation supports use in environmentally sensitive applications.Reduced maintenance — Ashle.. |
|||
Saybolt Viscosity at 210°F | 60 SUS | 60 SUS | |
ChevronTexaco Dura-Lith® NLGI 0 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Saybolt Viscosity at 210°F | 60 SUS | 60 SUS | |
ChevronTexaco Dura-Lith® NLGI 00 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Saybolt Viscosity at 210°F | 60 SUS | 60 SUS | ASTM D445 |
ChevronTexaco Cetus® PAO 68 Texaco Cetus PAO oils deliver value through:Long lubricant life in high temperature operations — Outstanding thermal and oxidation stability.Extended machinery life and increased compressor efficie.. |
|||
Saybolt Viscosity at 210°F | 60 SUS | 60 SUS | |
ChevronTexaco SAE 30 Transmission and Drive Train TO-4 Oil Texaco Transmission and Drive Train TO-4 Oils deliver value through:Longer equipment life — Special additives protect metal surfaces against scuffing and wear even under severe operating conditions.. |