Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 808 SUS | 808 SUS | |
ConocoPhillips Hydroclear® MV150 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |