Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Saybolt Viscosity at 100°F = 2565 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 2565 SUS
2565 SUS
ChevronTexaco ParaMount™ ELV Paraffinic Process Oil
FeaturesChevron ParaMount ELV Paraffinic Process Oil offers all the advantages of a bright stock including low weight loss and excellent solubility.ELV is exceptional because of its very light color..