Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 1946 SUS | 1946 SUS | Base Oil Property |
ConocoPhillips 1 Milube® Grease 2100 NLGI No. 1 Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic .. |
|||
Saybolt Viscosity at 100°F | 1946 SUS | 1946 SUS | Base Oil Property |
ConocoPhillips 1 Milube® Grease 2100T NLGI No. 1 Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic .. |