Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 166 SUS | 166 SUS | Base Oil Property |
ConocoPhillips Syncon® HP Synthetic Grease NLGI No. 1 Description: Conoco Syncon HP Synthetic Grease is a high-quality, synthetic polyalphaolefin (PAO) lithium grease developed to provide exceptional protection and corrosion resistance for bearings and.. |