Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Permeability | 1600 cm3 mil/(m2 day atm) | 103 cm3 mil/(100 in2 day atm) | |
Topas Advanced Polymers TOPAS® 9903D-10 Cyclic Olefin Copolymer (COC) TOPAS® 9903D-10 is a very low glass transition temperature (Tg=33°C) film extrusion grade. It is designed to deliver high shrinkage at low temperatures in shrink packaging applications. It is a mo.. |