Physical Properties | Metric | English | Comments |
---|---|---|---|
API Gravity | 31.6 ° | 31.6 ° | |
ChevronTexaco 40 White Oil Texaco White Oils 40 delivers value through:Nonstaining — Colorless, odorless, tasteless and nonstaining. The purity of Texaco White Oil 40 makes it the preferred choice for applications calling fo.. |
|||
API Gravity | 31.6 ° | 31.6 ° | |
ChevronTexaco 68 AW Hydraulic Oil Texaco AW Hydraulic Oils deliver value through:High oxidation stability — Longer service life than with conventional lubricants in high pressure service.Rust and corrosion protection — Gives excel.. |
|||
API Gravity | 31.6 ° | 31.6 ° | |
ChevronTexaco ISO 68 Hydraulic Oil AW FeaturesChevron Hydraulic Oils AW are designed to give excellent hydraulic pump protection. They are formulated with refined paraffinic base oils. They provide excellent antiwear protection, oxidati.. |
|||
API Gravity | 31.6 ° | 31.6 ° | |
ChevronTexaco Rando® HD 68 Texaco Rando HD oils deliver value through:Longer equipment life — Special antiwear additive package reduces wear by protecting surfaces when load causes breakdown of the lubricant film.Reduced dow.. |
|||
API Gravity | 31.6 ° | 31.6 ° | |
ChevronTexaco Rykon® ISO 68 Oil AW FeaturesChevron Rykon Oils AW are designed to give maximum hydraulic pump protection.Chevron Rykon Oils AW are formulated with ISOSYN® base stocks.They provide excellent antiwear protection, oxidat.. |
|||
API Gravity | 31.6 ° | 31.6 ° | |
ChevronTexaco Superla® 21 White Oil FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.These nearly ch.. |