Physical Properties | Metric | English | Comments |
---|---|---|---|
API Gravity | 27.5 ° | 27.5 ° | |
ChevronTexaco 120 Aircraft Engine Oils Texaco Aircraft Engine Oils deliver value through:Use of high quality straight mineral oil with low volatilityRigid quality control through production in an ISO 9002 certified facilityProvide a stab.. |
|||
API Gravity | 27.5 ° | 27.5 ° | |
ChevronTexaco Aero SAE 60/Grade 120 Engine Oil Uncompounded FeaturesChevron Aero Engine Oils Uncompounded are a blend of high quality base oil, with small amounts of viscosity modifier for improved fluidity at cold temperatures, antioxidant, and antifoam age.. |
|||
API Gravity | 27.5 ° | 27.5 ° | |
ChevronTexaco HDAX® SAE 40 LFG Gas Engine Oil FeaturesChevron HDAX LFG Gas Engine Oil is a premium quality, medium ash, dispersant/detergent type gas engine oil formulated especially for landfill gas and sour gas application.It is formulated wi.. |
|||
API Gravity | 27.5 ° | 27.5 ° | |
ChevronTexaco ISO 320 AIO FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring .. |
|||
API Gravity | 27.5 ° | 27.5 ° | ASTM D287 |
ChevronTexaco Regal® 320 R&O Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high.. |
|||
API Gravity | 27.5 ° | 27.5 ° | |
ConocoPhillips HD Fleet™ 149 Engine Oil SAE 50 Description: Conoco HD Fleet 149 Engine Oil is a high-quality, low ash API CF-2 single-grade oil recommended for high-output, two-stroke cycle diesel engines. It is formulated primarily for DD Serie.. |
|||
API Gravity | 27.5 ° | 27.5 ° | |
ConocoPhillips Hydroclear® 50 Power-D E.O. 50 Description: Conoco Hydroclear Power-D Engine Oil, formulated from Conoco's premium hydrocracked base stock, protects diesel and gasoline engines against wear, deposits, varnish, rust and corros.. |
|||
API Gravity | 27.5 ° | 27.5 ° | ASTM D287 |
ChevronTexaco Regal® 320 Texaco Regal oil delivers value through:Long lubricant life provided by good natural thermal and oxidation stability.Good demulsibility, which assures good lubricant, film strength and reduced wear .. |