Physical Properties Metric English Comments
Oxidative Induction Time (OIT) >= 80 min
>= 80 min
ASTM D3985
LyondellBasell Plexar® PX2246 Extrudable Tie-Layer Resin - Anhydride Modified HDPE
General DescriptionPlexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resin..