Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxidative Induction Time (OIT) | >= 80 min | >= 80 min | ASTM D3985 |
LyondellBasell Plexar® PX2246 Extrudable Tie-Layer Resin - Anhydride Modified HDPE General DescriptionPlexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resin.. |