Physical Properties Metric English Comments
Pore Size 0.00400 microns
0.000157 mil
Median Pierce adsorption mesopore, based on surface area
Zircar Zirconia ZYBF-4 Zirconia Bulk Fiber Insulation
Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed ..
Pore Size 0.00400 microns
0.000157 mil
Average
Corning Vycor® 7930 Porous Glass
Open cell porous glass which exhibits excellent moisture absorbing properties ("thirsty"). It is mechanically hard and strong, nondusting, nonflaking, and chemically inert. These properties allow ..
Pore Size 0.00400 microns
0.000157 mil
Median Pierce adsorption mesopore, based on surface area
Zircar Zirconia ZYBF-4 Zirconia Bulk Fiber Insulation
Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed ..