Polymer Property : Apparent Bulk Density = 0.0318 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.0220 - 0.880 g/cc
0.000795 - 0.0318 lb/in³
Average value: 0.262 g/cc Grade Count:24
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu..