Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.550 - 0.750 g/cc | 0.0199 - 0.0271 lb/in³ | ISO 60 |
Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |
|||
Apparent Bulk Density | 0.550 - 0.750 g/cc | 0.0199 - 0.0271 lb/in³ | ISO 60 |
Raschig Group MELOPAS® 6605 MP Melamine Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be.. |
|||
Apparent Bulk Density | 0.550 - 0.750 g/cc | 0.0199 - 0.0271 lb/in³ | ISO 60 |
Raschig Group MELOPLAS® 152 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |
|||
Apparent Bulk Density | 0.550 - 0.750 g/cc | 0.0199 - 0.0271 lb/in³ | ISO 60 |
Raschig Group MELOPLAS® 152.7 MF Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically.. |
|||
Apparent Bulk Density | 0.550 - 0.750 g/cc | 0.0199 - 0.0271 lb/in³ | ISO 60 |
Raschig Group MELOPLAS® 181 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc.. |
|||
Apparent Bulk Density | 0.550 - 0.750 g/cc | 0.0199 - 0.0271 lb/in³ | ISO 60 |
Raschig Group MELOPLAS® 181.5 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis.. |
|||
Apparent Bulk Density | 0.550 - 0.750 g/cc | 0.0199 - 0.0271 lb/in³ | ISO 60 |
Raschig Group MELOPLAS® 182 MF Wood flour-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in dark colors. Improved dimensional stability and electrical properties as compared with MP 180, high surf.. |
|||
Apparent Bulk Density | 0.550 - 0.750 g/cc | 0.0199 - 0.0271 lb/in³ | ISO 60 |
Raschig Group MELOPLAS® 183 MF Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18.. |
|||
Apparent Bulk Density | 0.550 - 0.750 g/cc | 0.0199 - 0.0271 lb/in³ | ISO 60 |
Raschig Group MELOPLAS® 2500 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |
|||
Apparent Bulk Density | 0.670 - 0.750 g/cc | 0.0242 - 0.0271 lb/in³ | IS 867-1963 |
Amity Thermosets ATI 172 Phenolic Molding Organic and inorganic Filler, Injection Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackVery soft flow .. |
|||
Apparent Bulk Density | 0.700 - 0.750 g/cc | 0.0253 - 0.0271 lb/in³ | IS 867-1963 |
Amity Thermosets ATS 1612 Phenolic Molding Nylon, inorganic, and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Apparent Bulk Density | 0.700 - 0.750 g/cc | 0.0253 - 0.0271 lb/in³ | IS 867-1963 |
Amity Thermosets ATS 1613-G Phenolic Molding Nylon and inorganic Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Apparent Bulk Density | 0.550 - 0.750 g/cc | 0.0199 - 0.0271 lb/in³ | ISO 60 |
Raschig Group MELOPLAS® 180 MF Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing .. |