Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 1.77 g/cc | 0.0639 lb/in³ | |
Poco Graphite ACF-10Q Industrial Grade Graphite POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr.. |
|||
Apparent Bulk Density | 1.77 g/cc | 0.0639 lb/in³ | |
Poco Graphite DFP Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Apparent Bulk Density | 1.77 g/cc | 0.0639 lb/in³ | |
Poco Graphite Glassmate® LT Graphite In very high wear situations, LT, with a hardness rating higher than GM material, will resist wear longer. |
|||
Apparent Bulk Density | 1.77 g/cc | 0.0639 lb/in³ | |
Poco Graphite SCF Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Apparent Bulk Density | 1.77 g/cc | 0.0639 lb/in³ | |
Poco Graphite SCF-2 Ion Implant Grade Graphite An economic alternative to DFP-3-2, this 5-micron material is harder than DFP-3-2 and has high strengths without reduced porosity. |
|||
Apparent Bulk Density | 1.77 g/cc | 0.0639 lb/in³ | |
Poco Graphite HPD Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Apparent Bulk Density | 1.77 g/cc | 0.0639 lb/in³ | |
Poco Graphite ZEE-2 Ion Implant Grade Graphite ZEE is a hard, wear-resistant material. This next generation ion implant material offers improved performance through the entire range of low to high-energy implants. POCO ZEE is high-purity, isotro.. |