Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | ASTM D4894 |
3M Dyneon™ TFM™ 1600 Modified PTFE Powder
(discontinued **) Type III, gr. 2 PTFE. Dyneon TFM 1600 PTFE is a free-flowing powder for compression molding, isostatic molding, automatic molding, and ram extrusion. Dyneon™ TFM™ 1600 PTFE is a second-generatio.. |
|||
Apparent Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | ASTM D4894 |
3M Dyneon™ 1641 PTFE Powder
(discontinued **) Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Apparent Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | ASTM D4894 |
3M Dyneon™ 1645 PTFE Powder
(discontinued **) Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Apparent Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U.. |
|||
Apparent Bulk Density | 0.830 - 0.930 g/cc | 0.0300 - 0.0336 lb/in³ | Limit; M2E-72-015 |
Indorama Ventures Mexico Polyclear™ Plus 1111 PET Resin Description: La resina Polyclear® Plus PET 1111 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g. Los envases fabricados con este material tienen un.. |
|||
Apparent Bulk Density | 0.830 - 0.930 g/cc | 0.0300 - 0.0336 lb/in³ | Limit; M2E-72-015 |
Indorama Ventures Mexico Polyclear™ Preserve 2201 PET Resin Description: La resina Polyclear® Preserve PET 2201 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g y esta disenada para ofrecer un redimiento supe.. |
|||
Apparent Bulk Density | 0.830 - 0.930 g/cc | 0.0300 - 0.0336 lb/in³ | 60 pellets/g, Limit; M2E-72-015 |
Indorama Ventures Mexico Polyclear™ Refresh 1101 PET Resin Description: La resina Polyclear® Refresh PET 1101 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g. Los envases fabricados con este material tienen.. |
|||
Apparent Bulk Density | 0.830 - 0.950 g/cc | 0.0300 - 0.0343 lb/in³ | Average value: 0.890 g/cc Grade Count:5 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |