Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.750 - 0.900 g/cc | 0.0271 - 0.0325 lb/in³ | ISO 60 |
Raschig Group 5553 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Apparent Bulk Density | 0.750 - 0.900 g/cc | 0.0271 - 0.0325 lb/in³ | ISO 60 |
Raschig Group 5562 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Apparent Bulk Density | 0.750 - 0.900 g/cc | 0.0271 - 0.0325 lb/in³ | ISO 60 |
Raschig Group 5563 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Apparent Bulk Density | 0.750 - 0.950 g/cc | 0.0271 - 0.0343 lb/in³ | ISO 60 |
Raschig Group AMPLA® 2000 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve.. |
|||
Apparent Bulk Density | 0.750 - 1.00 g/cc | 0.0271 - 0.0361 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 2100 UP Polyester Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta.. |
|||
Apparent Bulk Density | 0.750 - 1.00 g/cc | 0.0271 - 0.0361 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 2200 UP Polyester Organically filled polyester molding compound. Low post-shrinkage, good electrical values and mechanical properties, high surface quality and good color stability (non-yellowing). This product meets.. |
|||
Apparent Bulk Density | 0.750 - 0.950 g/cc | 0.0271 - 0.0343 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 4385 UP Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very high arc resistance, very high mechanical values. This product meets the allowed upper limits for heavy.. |
|||
Apparent Bulk Density | 0.750 - 1.00 g/cc | 0.0271 - 0.0361 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 4802 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Apparent Bulk Density | 0.750 - 0.950 g/cc | 0.0271 - 0.0343 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 4806 UP Glass-fiber reinforced polyester molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values, better performance values compared to UP 80.. |
|||
Apparent Bulk Density | 0.750 - 1.00 g/cc | 0.0271 - 0.0361 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 802 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up.. |
|||
Apparent Bulk Density | 0.750 - 1.00 g/cc | 0.0271 - 0.0361 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 804 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m.. |
|||
Apparent Bulk Density | 0.750 - 1.00 g/cc | 0.0271 - 0.0361 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 8601 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren.. |
|||
Apparent Bulk Density | 0.750 - 1.00 g/cc | 0.0271 - 0.0361 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 8602 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng.. |
|||
Apparent Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | DIN 53 466 |
3M Dyneon™ TF 4215 PTFE 25% Electrocarbon Filled
(discontinued **) Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon. |
|||
Apparent Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | DIN 53 466 |
3M Dyneon™ TFM™ 4215 Modified PTFE, 25% Electrocarbon Filled
(discontinued **) Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon. |
|||
Apparent Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | DIN 53 466 |
3M Dyneon™ TF 4303 PTFE 15% Graphite Filled
(discontinued **) Type II PTFE. Applications include sliding surfaces, bearings, seals/gaskets.Data provided by Dyneon. |
|||
Apparent Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 2774 Phenolic Formaldehyde Resin, Dishwasher Proof, Improved Electrical Properties, Low Shrinkage, UL Listed Phenolic molding compound, inorganically filled, glass fiber reinforced, increased dimensional stability, averaged notched impact strength, average heat resistance, improved electrical properties, U.. |
|||
Apparent Bulk Density | >= 0.750 g/cc | >= 0.0271 lb/in³ | Compacted; ISO 60 |
SolVin 561SF Vinyl Chloride - Vinyl Acetate copolymer Paste - filler Made by suspension polymerization.
APPLICATIONS
This resin has been especially developed for automotive mastics.Information provided by SolVin. |
|||
Apparent Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | |
Sumitomo Bakelite North America 52-01 Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG.Inf.. |
|||
Apparent Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | |
Sumitomo Bakelite North America 52-70-70-VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948 Type.. |
|||
Apparent Bulk Density | 0.750 - 0.850 g/cc | 0.0271 - 0.0307 lb/in³ | IS 867-1963 |
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Apparent Bulk Density | 0.750 - 0.850 g/cc | 0.0271 - 0.0307 lb/in³ | IS 867-1963 |
Amity Thermosets ATS 134 Phenolic Molding Inorganic, graphite Filler, Compression Molded Characteristics: Low coefficient of frictionSelf lubricating ( graphite modified )Good thermal conductivityGood glide propertiesNot suitable for electrical applicationColor- black gray Soft/medium f.. |
|||
Apparent Bulk Density | 0.750 - 0.850 g/cc | 0.0271 - 0.0307 lb/in³ | IS 867-1963 |
Amity Thermosets ATS 158 Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:Ammonia free Increased CTI High electrical insulation properties High mechanical strength Temperature stability (230 0 C) Color-black Medium flow Applications:Switchgear componentCom.. |
|||
Apparent Bulk Density | 0.750 - 0.840 g/cc | 0.0271 - 0.0303 lb/in³ | IS 867-1963 |
Amity Thermosets ATS 131 Phenolic Molding Organic and graphite Filler, Compression Molded Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti.. |
|||
Apparent Bulk Density | 0.750 - 0.900 g/cc | 0.0271 - 0.0325 lb/in³ | ISO 60 |
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc.. |
|||
Apparent Bulk Density | 0.750 - 0.900 g/cc | 0.0271 - 0.0325 lb/in³ | ISO 60 |
Raschig Group 5557 DAP
(discontinued **) Glass fiber-reinforced and inorganically filled diallylphthalate molding compound (DAP) in various colors. Good mechanical strength together with retention of high electrical properties under hot h.. |