Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ASTM D1895 |
Nilit Polynil® P-240 General Purpose Nylon 66 High Viscosity. Moisture content |
|||
Apparent Bulk Density | 0.700 - 0.850 g/cc | 0.0253 - 0.0307 lb/in³ | ISO 60 |
Raschig Group 2567 AMC Glass fiber-reinforced and inorganically filled polyester molding compound (UP) in various colors. Outstanding mechanical strength similar to BMC/SMC, very good electrical isolation properties and .. |
|||
Apparent Bulk Density | 0.700 - 0.850 g/cc | 0.0253 - 0.0307 lb/in³ | ISO 60 |
Raschig Group 2572 AMC Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin.. |
|||
Apparent Bulk Density | 0.700 - 0.850 g/cc | 0.0253 - 0.0307 lb/in³ | ISO 60 |
Raschig Group 6501 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Apparent Bulk Density | 0.700 - 0.850 g/cc | 0.0253 - 0.0307 lb/in³ | ISO 60 |
Raschig Group 6502 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Apparent Bulk Density | 0.700 - 0.850 g/cc | 0.0253 - 0.0307 lb/in³ | ISO 60 |
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Apparent Bulk Density | 0.700 - 0.850 g/cc | 0.0253 - 0.0307 lb/in³ | ISO 60 |
Raschig Group 6552 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Apparent Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | ISO 60 |
Raschig Group AMPLA® 7250 melamine-modified polyester Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow.. |
|||
Apparent Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | ISO 60 |
Raschig Group AMPLA® 7500 melamine-modified polyester Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta.. |
|||
Apparent Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | ISO 60 |
Raschig Group DECAL® 666/8 Phenolic Glass-fiber reinforced phenolic molding compound with mineral fillers. High heat resistance, reduced mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This prod.. |
|||
Apparent Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | ISO 60 |
Raschig Group DECAL® 937 Phenolic Mica reinforced phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (W.. |
|||
Apparent Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | ISO 60 |
Raschig Group SURAPLAST 54 UPA Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Apparent Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Hexion Bakelite™ MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
(d Melamine/phenolic molding compound, inorganically filled, glass fiber reinforced, good temperature stability, high level of mechanical properties, copper adhesive, flammability UL 94/V-0/1.6 mm (not.. |
|||
Apparent Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 2535 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof
(discontinued ** Phenolic molding compound, inorganically/organically filled, average heat resistant, steam resistant, dish washer proof, high surface quality.Application areas: Fittings for ovens and dishwashers, t.. |
|||
Apparent Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | Apparent density per ASTM D1895 |
Plenco 4759 Phenolic, Granular, Injection Molded
(discontinued **) Two-stage Phenolic. PLENCO 04759 is a black, two stage, medium heat resistant phenolic molding compound. It has excellent molded finish and possesses good electrical properties. It is used in appli.. |
|||
Apparent Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ASTM D1895 |
Plenco 501 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 501 is a two-stage, mineral and flock-filled phenolic molding compound designed for use in heat resistant and electrical applications. It is designed for elevated temperature exposure for e.. |
|||
Apparent Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ASTM D1895 |
Plenco 506 Black Heat Resistant Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok 506 is a two-stage, mineral-filled phenolic molding compound. It is formulated for automotive ashtrays and for appliance applications such as utensil handles receiving repeated exposure to .. |
|||
Apparent Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ASTM D1895 |
Plaslok 506 Black Heat Resistant Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 506 is a two-stage, mineral-filled ph.. |
|||
Apparent Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | Tap density |
Momentive Performance Materials AC-6028 Boron Nitride (BN) Powder Grade AC-6028 consists of agglomerated particles of hexagonal Boron Nitride (BN) with a mean particle size between 100 and 150µ. It exhibits the unique properties of BN in a form readily used in.. |
|||
Apparent Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ASTM D-1875 |
Lubrizol Advanced Materials Pearlthane® MB-9005 Thermoplastic Polyurethane Elastomer Pearlthane® MB-9005 is a TPU-based color masterbatch, supplied in the form of homogenously black colored pellets. It is specially intended for coloring TPUs (either polyester or polyether-based).. |
|||
Apparent Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | Apparent packing density; ISO 1068 |
SolVin 266SC Polyvinyl Chloride Pastes - filler Polymers Made by suspension polymerization.
APPLICATIONS
Filler polymer for plastisols.
CHARACTERISTICS
SolVin 266SC is a suspension resin with very low porosity, small particle size and a very low amount of.. |
|||
Apparent Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | |
Cosmic Plastics K31 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Apparent Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | TRM-37 |
Tipco Tipcolite® TG 618 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Apparent Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | TRM-37 |
Tipco Tipcolite® THD 121 Phenolic Compound, Wood Flour, having Medium Flow & High Strength Medium Flow Phenolic Compound, Reinforced with Wood FlourApplications: Electrical & ElectronicsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India... |
|||
Apparent Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | TRM-37 |
Tipco Tipcolite® VASW 150 Phenolic Compound, Glass Fibers & Minerals, Medium-Soft Flow & High Strength |
|||
Apparent Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ASTM D1895 |
Ashley Polymers Ashlene® 531 Nylon 66 For Monofilament spinning/super dry.Data provided by the manufacturer |
|||
Apparent Bulk Density | 0.700 - 0.750 g/cc | 0.0253 - 0.0271 lb/in³ | IS 867-1963 |
Amity Thermosets ATS 1613-G Phenolic Molding Nylon and inorganic Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Apparent Bulk Density | 0.700 - 1.30 g/cc | 0.0253 - 0.0470 lb/in³ | Average value: 0.950 g/cc Grade Count:5 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Apparent Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 4010 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage
(disconti Glass fiber reinforced and inorganically filled molding compound. High heat resistance, reduced molding shrinkage, good chemical resistance and mechanical properties.Application areas: Switch housi.. |
|||
Apparent Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ASTM D1895 |
Plaslok 501 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 501 is a two-stage, mineral and flock.. |