Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.510 g/cc | 0.0184 lb/in³ | ASTM D4894 |
Solvay Specialty Polymers Algoflon® 15GL+3Mos PTFE; Glass Fiber/Molybdenum Disulphide Filled
(discontinued ** Data provided by the manufacturer.15 wt.% Glass Fiber + 3 wt.% MoS2. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric pro.. |
|||
Apparent Bulk Density | 0.510 g/cc | 0.0184 lb/in³ | DIN 53 466 |
3M Dyneon™ TF 2024 PTFE Paste Extrusion Powder
(discontinued **) Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 500. Average particle size 500µm. Used for unsintered tapes and sealing cords.Dyneon offers a family of PTFE fine powder .. |
|||
Apparent Bulk Density | 0.510 g/cc | 0.0184 lb/in³ | DIN 53 466 |
3M Dyneon™ TF 2025 PTFE Paste Extrusion Powder
(discontinued **) Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 300. Average particle size 500µm. Used for liners.Dyneon offers a family of PTFE fine powder paste extrusion resins. Thes.. |
|||
Apparent Bulk Density | 0.510 g/cc | 0.0184 lb/in³ | DIN 53 466 |
3M Dyneon™ TF 2071 PTFE Paste Extrusion Powder
(discontinued **) Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 1600. Average particle size 500 µm. Used for tubing, wire/cable insulation, 'spaghetti tubing' production.Dyneon offers a.. |
|||
Apparent Bulk Density | 0.510 g/cc | 0.0184 lb/in³ | ASTM D4894 |
Solvay Specialty Polymers Algoflon® 25GL PTFE; Glass Fiber Filled
(discontinued **) Data provided by the manufacturer.25 wt.% Glass Fiber. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almos.. |
|||
Apparent Bulk Density | 0.510 - 0.570 g/cc | 0.0184 - 0.0206 lb/in³ | ISO 60:1977 |
BorsodChem ONGROVIL S-465 Suspension PVC-Resin S-465 is a suspension type PVC homopolymer of medium molecular mass. It is characterized by a porous particle structure, a narrow range of particle size and a relatively high apparent density. It re.. |
|||
Apparent Bulk Density | 0.510 - 0.570 g/cc | 0.0184 - 0.0206 lb/in³ | ISO 60:1977 |
BorsodChem ONGROVIL S-5067 Suspension PVC-Resin S-5067 is a suspension type PVC homopolymer of medium molecular mass. It is characterized by a porous particle structure, a narrow range of particle size and a relatively high apparent density. It r.. |