Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.100 - 0.200 g/cc | 0.00361 - 0.00723 lb/in³ | |
NanoAmor 90%, OD/ID: 10-30/3-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Apparent Bulk Density | 0.100 g/cc | 0.00361 lb/in³ | |
NanoAmor 95%, OD/ID: 60-100/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Apparent Bulk Density | 0.100 g/cc | 0.00361 lb/in³ | |
NanoAmor 95%, OD/ID: 10-30/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Apparent Bulk Density | 0.100 g/cc | 0.00361 lb/in³ | |
NanoAmor 95%, OD/ID: 40-60/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Apparent Bulk Density | 0.100 g/cc | 0.00361 lb/in³ | |
Cytec Thornel® Mat VMC Carbon Fiber Data provided by the manufacturer, Amoco Performance Products, Inc.Prepared by sectioning mat VMA into cubes ~ 0.5x0.5x1.0 in. VMC can be heterogeneously dispersed in matrix materials and thus enha.. |