Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.0220 g/cc | 0.000795 lb/in³ | On a discontinuous pre-expander |
Polimeri Europa Extir® E 2000 AE Expandable Polystyrene
(discontinued **) Extir E 2000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Thi.. |
|||
Apparent Bulk Density | 0.0220 g/cc | 0.000795 lb/in³ | On a continuous pre-expander after one expansion |
Polimeri Europa Extir® E 3000 AE Expandable Polystyrene
(discontinued **) Extir E 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. T.. |
|||
Apparent Bulk Density | 0.0220 g/cc | 0.000795 lb/in³ | Free-rise Density, Bayer test |
Covestro Bayfill® EA 2001 Polyurethane Energy-Absorbing Semi-Rigid Foam, Friable Grade, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Apparent Bulk Density | 0.0220 g/cc | 0.000795 lb/in³ | On a continuous pre-expander after one expansion |
Polimeri Europa Extir® EH 5000 Expandable Polystyrene Extir EH 5000 is an expandable polystyrene in the form of spherical beads of medium-large particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. This grade i.. |
|||
Apparent Bulk Density | 0.0220 - 0.880 g/cc | 0.000795 - 0.0318 lb/in³ | Average value: 0.262 g/cc Grade Count:24 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |