Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.950 - 1.10 g/cc | 0.0343 - 0.0397 lb/in³ | ISO 60 |
Raschig Group 3536 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Apparent Bulk Density | 0.900 - 1.10 g/cc | 0.0325 - 0.0397 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 4566 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |