Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.700 - 0.850 g/cc | 0.0253 - 0.0307 lb/in³ | ISO 60 |
Raschig Group 2557 AMC Polyester Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low .. |
|||
Apparent Bulk Density | 0.700 - 0.850 g/cc | 0.0253 - 0.0307 lb/in³ | ISO 60 |
Raschig Group 2567 AMC Glass fiber-reinforced and inorganically filled polyester molding compound (UP) in various colors. Outstanding mechanical strength similar to BMC/SMC, very good electrical isolation properties and .. |
|||
Apparent Bulk Density | 0.700 - 0.850 g/cc | 0.0253 - 0.0307 lb/in³ | ISO 60 |
Raschig Group 2572 AMC Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin.. |
|||
Apparent Bulk Density | 0.700 - 0.850 g/cc | 0.0253 - 0.0307 lb/in³ | ISO 60 |
Raschig Group 6501 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Apparent Bulk Density | 0.700 - 0.850 g/cc | 0.0253 - 0.0307 lb/in³ | ISO 60 |
Raschig Group 6502 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Apparent Bulk Density | 0.700 - 0.850 g/cc | 0.0253 - 0.0307 lb/in³ | ISO 60 |
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Apparent Bulk Density | 0.700 - 0.850 g/cc | 0.0253 - 0.0307 lb/in³ | ISO 60 |
Raschig Group 6552 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Apparent Bulk Density | 0.650 - 0.850 g/cc | 0.0235 - 0.0307 lb/in³ | ISO 60 |
Raschig Group SURAPLAST UPA 63 UP Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Apparent Bulk Density | 0.700 - 0.850 g/cc | 0.0253 - 0.0307 lb/in³ | IS 867-1963 |
Amity Thermosets ATE 183 M Phenolic Molding Mica and organic Filler, Compression Molded Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl.. |
|||
Apparent Bulk Density | 0.750 - 0.850 g/cc | 0.0271 - 0.0307 lb/in³ | IS 867-1963 |
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Apparent Bulk Density | 0.750 - 0.850 g/cc | 0.0271 - 0.0307 lb/in³ | IS 867-1963 |
Amity Thermosets ATS 134 Phenolic Molding Inorganic, graphite Filler, Compression Molded Characteristics: Low coefficient of frictionSelf lubricating ( graphite modified )Good thermal conductivityGood glide propertiesNot suitable for electrical applicationColor- black gray Soft/medium f.. |
|||
Apparent Bulk Density | 0.750 - 0.850 g/cc | 0.0271 - 0.0307 lb/in³ | IS 867-1963 |
Amity Thermosets ATS 158 Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:Ammonia free Increased CTI High electrical insulation properties High mechanical strength Temperature stability (230 0 C) Color-black Medium flow Applications:Switchgear componentCom.. |
|||
Apparent Bulk Density | 0.700 - 0.850 g/cc | 0.0253 - 0.0307 lb/in³ | IS 867-1963 |
Amity Thermosets ATE 183 Phenolic Molding Mica and organic Filler, Compression Molded Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl.. |
|||
Apparent Bulk Density | 0.730 - 0.850 g/cc | 0.0264 - 0.0307 lb/in³ | IS 867-1963 |
Amity Thermosets ATO 159 Phenolic Molding Glass/ inorganic Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |