Apparent Bulk Density 0.500 - 0.820 g/cc
0.0181 - 0.0296 lb/in³
Average value: 0.663 g/cc Grade Count:6
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..