Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.620 - 0.690 g/cc | 0.0224 - 0.0249 lb/in³ | IS 867-1963 |
Amity Thermosets ATM 144 Phenolic Molding Organic Filler, Compression Molded Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane.. |