Polymer Property : Apparent Bulk Density = 0.577 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.545 - 0.577 g/cc
0.0197 - 0.0208 lb/in³
Average value: 0.569 g/cc Grade Count:4
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum ..
Apparent Bulk Density 0.449 - 0.577 g/cc
0.0162 - 0.0208 lb/in³
Average value: 0.534 g/cc Grade Count:9
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported ..