Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.950 - 1.10 g/cc | 0.0343 - 0.0397 lb/in³ | ISO 60 |
Raschig Group 3536 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Apparent Bulk Density | 0.950 - 1.05 g/cc | 0.0343 - 0.0379 lb/in³ | ISO 60 |
Raschig Group 4552 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi.. |
|||
Apparent Bulk Density | 0.950 - 1.05 g/cc | 0.0343 - 0.0379 lb/in³ | ISO 60 |
Raschig Group 4554 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi.. |