Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.800 - 0.950 g/cc | 0.0289 - 0.0343 lb/in³ | ISO 60 |
Raschig Group 2568 AMC Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s.. |
|||
Apparent Bulk Density | 0.800 - 1.00 g/cc | 0.0289 - 0.0361 lb/in³ | ISO 60 |
Raschig Group DECAL® 666/8/2B Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe.. |
|||
Apparent Bulk Density | 0.800 - 1.00 g/cc | 0.0289 - 0.0361 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 5000 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all.. |
|||
Apparent Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ISO 60 |
Hexion Bakelite™ EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
(dis Epoxy molding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical even at higher temperatures, very slight post shrinkage, increased media resistance, UL l.. |
|||
Apparent Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | |
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I.. |
|||
Apparent Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Durez® 23570 Phenolic, Compression Grade Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft.. |
|||
Apparent Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Durez® 23570 Phenolic, Injection Grade Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft.. |
|||
Apparent Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Compression Grade Durez 32633 Black Phenolic is a two-stage, glass filled, special purpose molding compound. It is designed for applications requiring high physical strengths, dimensional stability, and heat resista.. |
|||
Apparent Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Injection Grade Durez 32633 Black Phenolic is a two-stage, glass filled, special purpose molding compound. It is designed for applications requiring high physical strengths, dimensional stability, and heat resista.. |
|||
Apparent Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | |
Sumitomo Bakelite North America FS-10-VO-P Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI.. |
|||
Apparent Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | |
Cosmic Plastics E4930 Mineral & Glass Filled Epoxy Molding Compound, Encapsulated Grade Data provided by the manufacturer. |
|||
Apparent Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | |
Arkema Group Lacovyl® GA 6015 Vinyl Copolymer LACOVYL GA 6015 is a copolymer of vinyl chloride and vinyl acetate with a low molecular weight and a high acetate content prepared by suspension polymerization.Its main characteristics are : Vinyl a.. |
|||
Apparent Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D4894 |
Solvay Specialty Polymers Algoflon® S 121 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p.. |
|||
Apparent Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D4894 |
Solvay Specialty Polymers Algoflon® 50 INOX PTFE; Stainless Steel Filled
(discontinued **) Data provided by the manufacturer.50 wt.% Stainless Steel. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, a.. |
|||
Apparent Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ISO 60 |
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U.. |
|||
Apparent Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,.. |