Physical Properties Metric English Comments
Apparent Bulk Density 0.68 g/cc
0.025 lb/in³
ASTM D1895
Sumitomo Bakelite Durez® 152 Phenolic, Compression Grade
Durez 152 Phenolic is a two-stage, heat resistant/electrical molding material. It exhibits superior dimensional stability, good strength retention at elevated temperature and good molded appearance..
Apparent Bulk Density 0.68 g/cc
0.025 lb/in³
ASTM D1895
Sumitomo Bakelite Durez® 152 Phenolic, Injection Grade
Durez 152 Phenolic is a two-stage, heat resistant/electrical molding material. It exhibits superior dimensional stability, good strength retention at elevated temperature and good molded appearance..