Polymer Property : Apparent Bulk Density = 0.520 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Plenco Valite 697-A Novolac Phenolic, Granular, Compression Molded  (discontinued **)
This Valite product has been replaced by Plenco 7697. Data provided by Plenco.VALITE 697-A is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for ..
Apparent Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Plaslok 301 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 301 is a two-stage, woodflour and flo..
Apparent Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Solvay Specialty Polymers Catalyst CT/1 Polyolefin
Catalyst CT/1 is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Polidan® and Polidiemme® series c..
Apparent Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Solvay Specialty Polymers Catalyst CT/1-LR Polyolefin
Catalyst CT/1-LR is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Polidan® and Polidiemme® series..
Apparent Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Solvay Specialty Polymers Catalyst CT/1-LR UV Polyolefin
Catalyst CT/1-LR UV is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Polidan® and Polidiemme® se..
Apparent Bulk Density 0.520 g/cc
0.0188 lb/in³
ISO 60
SolVin 271GA Polyvinyl Chloride General Purpose - Plasticized
Made by suspension polymerization. APPLICATIONS Extrusion : - plasticized and semi-rigid pipes for medical applications - plasticized film for blood bags Injection molding : plasticized and semi-rig..
Apparent Bulk Density 0.520 g/cc
0.0188 lb/in³
ISO 60
SolVin 271PC Polyvinyl Chloride General Purpose - Plasticized
Made by suspension polymerization. APPLICATIONS Extrusion : - plasticized and semi-rigid profiles and pipes - blowing of plasticized films Calendering : opaque or transparent, plasticized and semi-r..
Apparent Bulk Density 0.520 g/cc
0.0188 lb/in³
ISO 60
SolVin 557RB Copolymer of Vinyl Chloride and Vinyl Acetate
Made by suspension polymerization. APPLICATIONS Extrusion : sheets for vacuum-forming, for deformations of over 500 % Calendering : rigid sheets for deep thermoformingInformation provided by SolVin...
Apparent Bulk Density 0.520 g/cc
0.0188 lb/in³
ISO 60
SolVin 560RA Copolymer of Vinyl Chloride and Vinyl Acetate
Made by suspension polymerization. APPLICATIONS Extrusion : sheets for vacuum-forming, for deformations of over 500 % Calendering : rigid sheets for deep thermoformingInformation provided by SolVin...
Apparent Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Plenco 301 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok 301 is a two-stage, woodflour and flock-filled phenolic molding compound. It has broad molding latitude combined with good electrical properties and improved impact strength. It is particu..