Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.510 g/cc
0.0184 lb/in³
ASTM D4894
Solvay Specialty Polymers Algoflon® 15GL+3Mos PTFE; Glass Fiber/Molybdenum Disulphide Filled  (discontinued **
Data provided by the manufacturer.15 wt.% Glass Fiber + 3 wt.% MoS2. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric pro..
Apparent Bulk Density 0.510 g/cc
0.0184 lb/in³
DIN 53 466
3M Dyneon™ TF 2024 PTFE Paste Extrusion Powder  (discontinued **)
Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 500. Average particle size 500µm. Used for unsintered tapes and sealing cords.Dyneon offers a family of PTFE fine powder ..
Apparent Bulk Density 0.510 g/cc
0.0184 lb/in³
DIN 53 466
3M Dyneon™ TF 2025 PTFE Paste Extrusion Powder  (discontinued **)
Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 300. Average particle size 500µm. Used for liners.Dyneon offers a family of PTFE fine powder paste extrusion resins. Thes..
Apparent Bulk Density 0.510 g/cc
0.0184 lb/in³
DIN 53 466
3M Dyneon™ TF 2071 PTFE Paste Extrusion Powder  (discontinued **)
Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 1600. Average particle size 500 µm. Used for tubing, wire/cable insulation, 'spaghetti tubing' production.Dyneon offers a..
Apparent Bulk Density 0.510 g/cc
0.0184 lb/in³
ASTM D4894
Solvay Specialty Polymers Algoflon® 25GL PTFE; Glass Fiber Filled  (discontinued **)
Data provided by the manufacturer.25 wt.% Glass Fiber. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almos..
Apparent Bulk Density 0.510 - 0.570 g/cc
0.0184 - 0.0206 lb/in³
ISO 60:1977
BorsodChem ONGROVIL S-465 Suspension PVC-Resin
S-465 is a suspension type PVC homopolymer of medium molecular mass. It is characterized by a porous particle structure, a narrow range of particle size and a relatively high apparent density. It re..
Apparent Bulk Density 0.510 - 0.570 g/cc
0.0184 - 0.0206 lb/in³
ISO 60:1977
BorsodChem ONGROVIL S-5067 Suspension PVC-Resin
S-5067 is a suspension type PVC homopolymer of medium molecular mass. It is characterized by a porous particle structure, a narrow range of particle size and a relatively high apparent density. It r..