Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.370 g/cc | 0.0134 lb/in³ | Geon® STP 1169; Internal Method |
PolyOne Geon™ Specialty Suspension CG E 44 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® CG E44 is a homopolymer specialty suspension resin intended for use in lowering the gloss of extruded or plastisol parts. This resin provides low surface gloss and texturing effects for flexi.. |
|||
Apparent Bulk Density | 0.370 g/cc | 0.0134 lb/in³ | ASTM D4894 |
3M Dyneon™ 1750 PTFE Powder
(discontinued **) Type II PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a wide r.. |
|||
Apparent Bulk Density | 0.370 g/cc | 0.0134 lb/in³ | |
Lucobit Lucocell® PE3700 Cellulose Asphalt Additive Lucocell® PE3700 granules – cellulose additives for SMA –Stone Mastic Asphalt or Split Mastic Asphalt, which is used as finish for all road types. Due to their 3D structure, cellulose f.. |
|||
Apparent Bulk Density | 0.370 g/cc | 0.0134 lb/in³ | |
NOVA Chemicals Novapol® TR-0338-UG MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Apparent Bulk Density | 0.370 g/cc | 0.0134 lb/in³ | ASTM D4894 |
Solvay Specialty Polymers Algoflon® F6 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope.. |