Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.270 - 0.900 g/cc | 0.00975 - 0.0325 lb/in³ | Average value: 0.684 g/cc Grade Count:29 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Apparent Bulk Density | 0.270 g/cc | 0.00975 lb/in³ | |
Sumitomo Bakelite North America FS-4 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North A.. |
|||
Apparent Bulk Density | 0.270 g/cc | 0.00975 lb/in³ | |
Cosmic Plastics 224 Dacron Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |