Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.0400 g/cc | 0.00145 lb/in³ | |
NanoAmor 95%, OD/ID/L: 20-40/5-10 nm/1-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Apparent Bulk Density | 0.0400 - 0.0500 g/cc | 0.00145 - 0.00181 lb/in³ | |
NanoAmor 95%, OD/ID: 10-20/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Apparent Bulk Density | 0.0400 g/cc | 0.00145 lb/in³ | Free-rise Density, Bayer test |
Covestro Bayfill® 370 Polyurethane Semi-Rigid Foam, Polymeric Catalyst, Closed Pour, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Apparent Bulk Density | 0.0400 g/cc | 0.00145 lb/in³ | Free-rise Density, Bayer test |
Covestro Bayfill® 380 Polyurethane Semi-Rigid Foam, Polymeric Catalyst, Open Pour, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Apparent Bulk Density | 0.0400 g/cc | 0.00145 lb/in³ | Free-rise Density, Bayer test |
Covestro Bayfill® EA 4004 Polyurethane Energy-Absorbing Semi-Rigid Foam, Rigid Grade, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |