Physical Properties Metric English Comments
Apparent Bulk Density 0.0220 g/cc
0.000795 lb/in³
On a discontinuous pre-expander
Polimeri Europa Extir® E 2000 AE Expandable Polystyrene  (discontinued **)
Extir E 2000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Thi..
Apparent Bulk Density 0.0220 g/cc
0.000795 lb/in³
On a continuous pre-expander after one expansion
Polimeri Europa Extir® E 3000 AE Expandable Polystyrene  (discontinued **)
Extir E 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. T..
Apparent Bulk Density 0.0220 g/cc
0.000795 lb/in³
Free-rise Density, Bayer test
Covestro Bayfill® EA 2001 Polyurethane Energy-Absorbing Semi-Rigid Foam, Friable Grade, MDI-based 2-Component Liquid System
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Apparent Bulk Density 0.0220 g/cc
0.000795 lb/in³
On a continuous pre-expander after one expansion
Polimeri Europa Extir® EH 5000 Expandable Polystyrene
Extir EH 5000 is an expandable polystyrene in the form of spherical beads of medium-large particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. This grade i..
Apparent Bulk Density 0.0220 - 0.880 g/cc
0.000795 - 0.0318 lb/in³
Average value: 0.262 g/cc Grade Count:24
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu..
Copyright © lookpolymers.com All Rights Reserved