Physical Properties Metric English Comments
Apparent Bulk Density 0.0180 g/cc
0.000650 lb/in³
On a continuous pre-expander after one expansion
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene  (discontinued **)
Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or CFC. Extir D 30..
Apparent Bulk Density 0.0180 g/cc
0.000650 lb/in³
On a discontinuous pre-expander
Polimeri Europa Extir® EH 5000 Expandable Polystyrene
Extir EH 5000 is an expandable polystyrene in the form of spherical beads of medium-large particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. This grade i..
Apparent Bulk Density 0.0180 g/cc
0.000650 lb/in³
On a continuous pre-expander after one expansion
Polimeri Europa Extir® LN 2000 Expandable Polystyrene
Extir LN 2000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion..
Apparent Bulk Density 0.0180 g/cc
0.000650 lb/in³
On a continuous pre-expander after one expansion
Polimeri Europa Extir Leonardo A 2000 AE Expandable Polystyrene  (discontinued **)
Extir A 2000 AE is a flame retardant expandable polystyrene in the form of spherical beads of fine particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 200..