Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.0160 g/cc | 0.000578 lb/in³ | On a continuous pre-expander after one expansion |
Polimeri Europa Extir® LN 3000 Expandable Polystyrene Extir LN 3000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion.. |
|||
Apparent Bulk Density | 0.0160 g/cc | 0.000578 lb/in³ | On a discontinuous pre-expander |
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene
(discontinued **) Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or CFC. Extir D 30.. |
|||
Apparent Bulk Density | 0.0160 g/cc | 0.000578 lb/in³ | On a continuous pre-expander after one expansion |
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene
(discontinued **) Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext.. |
|||
Apparent Bulk Density | 0.0160 g/cc | 0.000578 lb/in³ | On a discontinuous pre-expander |
Polimeri Europa Extir® E 5000 AE Expandable Polystyrene
(discontinued **) Extir E 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, with a low pentane content as blowing agent. Extir does not contain CFC or H.. |
|||
Apparent Bulk Density | 0.0160 g/cc | 0.000578 lb/in³ | On a continuous pre-expander after two expansions |
Polimeri Europa Extir® EH 5000 Expandable Polystyrene Extir EH 5000 is an expandable polystyrene in the form of spherical beads of medium-large particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. This grade i.. |
|||
Apparent Bulk Density | 0.0160 g/cc | 0.000578 lb/in³ | On a discontinuous pre-expander |
Polimeri Europa Extir® LN 2000 Expandable Polystyrene Extir LN 2000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion.. |