Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 6.0 - 7.0 cP @Temperature 20.0 °C |
6.0 - 7.0 cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
DuPont Elvanol® 70-06 Polyvinyl Alcohol Fully Hydrolyzed General Purpose Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |
|||
Viscosity | 3.0 - 7.0 cP | 3.0 - 7.0 cP | |
Daikin NEOFLON ND-4 FEP Dispersion, Milky White NEOFLON FEP dispersions are fine-powder suspension. Two types are available: water based and organic solvent based. Since FEP has good flowability when melted, a continuous, pinhole-free film can .. |