Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 350 - 650 cP | 350 - 650 cP | 15% solution in MEK |
Lubrizol Advanced Materials Pearlstick® 45-40/05 Polycaprolactone based TPU
(discontinued **) TPUs for Solvent-based adhesivesApplications: DIY, AutomotiveInformation provided by Merquinsa |
|||
Viscosity | 350 - 650 cP @Temperature 23.0 °C |
350 - 650 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 320-LV Optically Opaque Epoxy Material Description: A two component, optically opaque epoxy adhesive designed for semiconductor and PCB applications in optoelectronic instrumentation and assemblies. A lower viscosity version of.. |
|||
Viscosity | 350 - 650 cP @Temperature 40.0 °C |
350 - 650 cP @Temperature 104 °F |
|
Abatron AboCast/AboCure 8109-10 2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro.. |
|||
Viscosity | 450 - 650 cP | 450 - 650 cP | blended |
Abatron AboCast 7802-1/AboCure 7804-3 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v.. |