Physical Properties Metric English Comments
Viscosity 200 - 375 cP
200 - 375 cP
Huntsman AroCy B-40S Prepolymer Bisphenol-A Dicyanate
Comments/Applications: Prepolymer of high purity bisphenol A dicyanate supplied @ 75% solids in MEK. High performance multi-layer printed wiring boards and multi-chip modules.Data provided by Ciba ..