Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 200 - 240 cP @Temperature 25.0 °C |
200 - 240 cP @Temperature 77.0 °F |
|
Esstech X-167-0000 Glass Ionomer Cement Liquid Our GIC liquid works well when paired with an alumino-fluoro-silicate glass filler. The combination leads to a quick, easy-to-use composite material. Listed on the Toxic Substance Control Act List... |
|||
Viscosity | 200 - 240 cP | 200 - 240 cP | Mixed Viscosity |
Aremco Corr-Paint™ CP2000 High Temperature Protective Coating Urethane, Carbon Filled These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h.. |