Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 190000 - 190000 cP @Temperature 280 - 280 °C |
190000 - 190000 cP @Temperature 536 - 536 °F |
Average value: 190000 cP Grade Count:2 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Viscosity | 190000 - 190000 cP @Shear Rate 1000 - 1000 1/s |
190000 - 190000 cP @Shear Rate 1000 - 1000 1/s |
Average value: 190000 cP Grade Count:2 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |