Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 900 - 1100 cP | 900 - 1100 cP | Liquid State |
Palm Labs Adhesives TURBO FUSE SERIES 160 LOW ODOR/LOW BLOOM (1000 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 160 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PAA-033 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PBA-031 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PBA-052 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PBA-055 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PBA-058 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PBA-064 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PPA-019 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PNA-157 Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 - 1100 cP | 700 - 1100 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1163 B (SIS) Linear Block Copolymer Description: Kraton D1163 B is a clear, linear block copolymer based on styrene and isoprene with a polystyrene content of 15%. It is supplied from South America in the physical form identified: Kra.. |
|||
Viscosity | 900 - 1100 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
900 - 1100 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2081126P2 Conductive Silver Polymer Paste This product is a thermoplastic screen printing ink, developed for use in membrane touch switch applications as well as counter electrode in electrochemical sensors and conductive tracks. It may be .. |
|||
Viscosity | 700 - 1100 cP | 700 - 1100 cP | |
Huntsman PY 258 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 185 to 196. Max color is 3.Comments/Applications: Provides excellent heat and chemical resistance especially in post bake or heat cured coatings. Chemically modified.. |
|||
Viscosity | 700 - 1100 cP | 700 - 1100 cP | |
Beijing Ranger Chem SM-815 Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 700 - 1100 cP | 700 - 1100 cP | |
Beijing Ranger Chem WSR615 Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 900 - 1100 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
900 - 1100 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2080415D2 Silver Counter Electrode Paste This product is a screen printable polymer paste designed as a counter electrode in electrochemical biosensors. This ink can be used in conjunction with our working carbon electrode ink C2030519P4, .. |