Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 800 - 1200 cP @Temperature 25.0 °C |
800 - 1200 cP @Temperature 77.0 °F |
|
Northstar Polymers PAA-071 Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 800 - 1200 cP @Temperature 25.0 °C |
800 - 1200 cP @Temperature 77.0 °F |
Uncured |
Permabond TA439 Toughened Acrylic Adhesive Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f.. |
|||
Viscosity | 800 - 1000 cP @Temperature 23.9 °C |
800 - 1000 cP @Temperature 75.0 °F |
|
TSE Industries EcoWIND® 100 Polyurethane Resin Filament Winding
(discontinued **) TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Viscosity | 800 cP | 800 cP | |
Resinlab® CYNERGY CA6402 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Viscosity | 800 cP | 800 cP | ASTM D2293 |
Fibre Glast Saf-T-Poxy 2410 / 2184 Epoxy
(discontinued **) Information provided by Fibre Glast Developments Corporation. |
|||
Viscosity | 800 - 1200 cP | 800 - 1200 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-632L TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Hydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for fo.. |
|||
Viscosity | 800 cP | 800 cP | Solution Viscosity; ASTM D455 |
Solvay Specialty Polymers Veradel® 3100P Polyethersulfone (PESU) Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with oth.. |
|||
Viscosity | 800 cP | 800 cP | Solution Viscosity; ASTM D455 |
Solvay Specialty Polymers Virantage® VW-10200 RP, RFP, RSFP Polyethersulfone (PESU) Virantage® VW-series functionalized polyethersulfones (r-PESU) are amorphous, high-temperature sulfone polymers featuring reactive end groups to enhance solubility and improve interfacial propert.. |
|||
Viscosity | 800 cP | 800 cP | Solution Viscosity; ASTM D455 |
Solvay Specialty Polymers Virantage® VW-10300 P, FP & SFP Polyethersulfone (PESU) Virantage® VW-10300 polyethersulfone (PESU) is a non-functionalized, high-temperature sulfone polymer powder. Three grades are offered: Virantage® VW-10300P, Virantage® VW-10300FP, and Vira.. |
|||
Viscosity | 800 - 1700 cP | 800 - 1700 cP | |
Solvay RHODOLINE® DF-665 Surfactant Description: Highly efficient mineral oil based defoamers for flat to gloss paints, quick process foam know down and high in-can persistency.Identification: OIL BASE DEFOAMERAvailable in: North Amer.. |
|||
Viscosity | 800 cP @Temperature 23.0 °C |
800 cP @Temperature 73.4 °F |
|
Master Bond EP29LP Low Exotherm, Low Viscosity Two Component Epoxy System Master Bond Polymer System EP29LP is a two component high performance epoxy resin system featuring low viscosity, long pot life and low exotherm. As an adhesive this versatile material will form bon.. |
|||
Viscosity | 800 - 1000 cP | 800 - 1000 cP | Part A |
Master Bond EP45HT-1 Adhesive Resists Exposure to Sterilization Description: Master Bond Polymer System EP45HT-1 is a remarkably fast curing, medium viscosity, two component epoxy compound formulated for high performance casting and bonding. It is 100% reactive .. |
|||
Viscosity | 800 cP @Temperature 25.0 °C |
800 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Eccobond® 24 Two-Component High Strength-Impact Resistant Epoxy Adhesive Emerson & Cuming 24 Eccobond® Two-Component High Strength-Impact Resistant Epoxy AdhesiveClear, low viscosity, room temperature curing, epoxy adhesive. Exhibits resilient bonds when joining dissimi.. |
|||
Viscosity | 800 cP | 800 cP | dynamic |
Dow Corning SE 1880 One-part, transparent gel, heat cure, low temperature capable.Information provided by Dow Corning |
|||
Viscosity | 800 cP | 800 cP | Dynamic |
Dow Corning SYL-OFF® PMCPSL 6 Crosslinker Minimizes mist at speeds up to 1600 m/min, good balance of cure and anchorage performance.Information provided by Dow Corning |
|||
Viscosity | 800 cP | 800 cP | dynamic |
Dow Corning SYL-OFF® SL 10 RELEASE MODIFIER Olefin-free; low viscosityInformation provided by Dow Corning |
|||
Viscosity | 800 - 5000 cP | 800 - 5000 cP | Dynamic |
Dow Corning XIAMETER® PMCPOFX-8040 Fluid Is chemically equivalent to DOW CORNING® 2-8040 POLYMER. Diaminofunctional silicone softener; suitable for formulation to a microemulsion that can be applied to all types of woven or knitted fabric.. |
|||
Viscosity | 800 cP @Temperature -25.0 °C |
800 cP @Temperature -13.0 °F |
Cold Crank |
ChevronTexaco 4R Unconventional Base Oil FeaturesChevron Unconventional Base Oils (UCBOs) are all hydroprocessed, highly refined paraffinic base oils of exceptional performance and purity.Relative to conventional hydroprocessed and solvent.. |
|||
Viscosity | 800 cP @Temperature 25.0 °C |
800 cP @Temperature 77.0 °F |
|
Cytec (Conap) RN-1000 / EA-117 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Viscosity | 800 - 1200 cP @Temperature 23.0 °C |
800 - 1200 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® CF6-2 High Temperature Epoxy Product Description: EPO-TEK® CF6-2 is a two component, high temperature and high Tg epoxy designed for fiber optic packaging. Advantages & Application Notes: The low viscosity nature allows for wi.. |
|||
Viscosity | 800 - 1600 cP @Temperature 23.0 °C |
800 - 1600 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® E4110 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E4110 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although other.. |
|||
Viscosity | 800 - 1200 cP | 800 - 1200 cP | |
Epoxyset Epoxibond EB-119M Unfilled Epoxy Adhesive A two-component,unfilled, low viscosity, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by.. |
|||
Viscosity | 800 cP | 800 cP | A Side |
ACC EP EF EPI Engineered Polymers Extra Flex Polyurea EP EF, Extra Flex Polyurea, “Powered by Reactamine® Technology, is a two component 100% solid Polyurea, with superior performance in industrial applications. EP EF displays extremely fast cure tim.. |
|||
Viscosity | 800 cP | 800 cP | |
Abatron AboCast 8503-3/AboCure 8503-3 Colorless Epoxy AboCast 8503-3/AboCure 8503-3 is a general purpose, medium speed, colorless epoxy casting compound with low viscosity. It has a good balance of properties with a fairly fast hardening. Suggested Use.. |
|||
Viscosity | 800 - 1000 cP | 800 - 1000 cP | Mixed Viscosity |
Aremco Corr-Paint™ CP2070 High Temperature Protective Coating Novolac-Epoxy, Pigment Only Filled Two part, novolac-epoxy with exceptional abrasion adn corrosion resistance for continuous operations to 300°F (150°C) and intermittent use to 400°F (204°C). |
|||
Viscosity | 800 cP | 800 cP | A Side |
ACC ReactAmine® EP 350 EPI Engineered Polymers Polyurea ReactAmine® EP-350 is a two component 100% solid Polyurea with superior performance in industrial applications. EP-350 displays extremely fast cure times with excellent adhesions to different subst.. |
|||
Viscosity | 800 - 1000 cP @Shear Rate 50.0 1/s, Temperature 25.0 °C |
800 - 1000 cP @Shear Rate 50.0 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2080815P1 Silver Flexographic Ink Silver conductor ink specifically designed for printing on to polymeric or paper substrates using flexographic printing. Ink can be printed at speeds up to 20m/min, with good line definition and go.. |
|||
Viscosity | 800 cP @Temperature 40.0 °C |
800 cP @Temperature 104 °F |
25% solution in DMAc; Internal Method |
Solvay Specialty Polymers Virantage® VW-10300 P, FP Polyethersulfone (PESU)
(Unverified Data**) Virantage® VW-10300 polyethersulfone (PESU) is a non-functionalized, high-temperature sulfone polymer powder. Two grades are offered: Virantage VW-10300P and Virantage VW-10300FP, providing two par.. |
|||
Viscosity | 800 - 1500 cP @Temperature 23.0 °C |
800 - 1500 cP @Temperature 73.4 °F |
|
Master Bond UV15-7SP4 Low Shrinkage, One Component, UV Curable System Master Bond Polymer System UV15-7SP4 is a one component, low viscosity UV system with flexibility. UV15-7SP4 has very little shrinkage when curing and has non-yellowing properties. It bonds well to .. |
|||
Viscosity | 800 - 1500 cP @Temperature 23.0 °C |
800 - 1500 cP @Temperature 73.4 °F |
|
Master Bond UV15-7SP4DC One Component, Dual Cured, Flexible UV System Master Bond Polymer System UV15-7SP4DC is a one component, optically clear, dual cured flexible UV and/or heat curable polymer system with extended service capability of -80°F to +250°F. It cures .. |