Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 67500 cP | 67500 cP | at 20 RPM |
Loctite® Depend© 330 Acrylic Bonding Adhesive Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. .. |
|||
Viscosity | 67500 cP | 67500 cP | Mixed - medium; Resin - 75,000 cP; Hardener - 7,000 cP |
Loctite® Durabond® E-60HP Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |